NB115Global product supply
NB-115
Related standardsCDA C19027、JASO JC400
ApplicationsTerminals for connector applications, switches, relays, IC lead frames, etc.
Copper alloy designed for connectors.
It features an improved balance of strength, springiness, and bendability over that of the NB-109.
NB-115 is a copper alloy with a superior balance of strength, springiness, and bendability.
It has excellent stress relaxation resistance.
It is well suited for downsizing, weight reduction, improving reliability, and cost reduction of electrical and electronic components.
It is registered as C19027 by the CDA (United States) and can be procured locally from Wieland in the United States.
Chemical composition
[wt%]
Ni | Sn | P | Cu | |
---|---|---|---|---|
Typical values | 0.9 | 1.55 | 0.07 | Rem. |
Physical properties
Melting point [℃] | 1080 |
---|---|
Density [g/cm3@20℃] | 8.9 |
Thermal expansion coefficient [10-6/K@20-300℃] |
17.0 |
Thermal conductivity [W/m・K@20℃] |
147 |
Electrical conductivity [%IACS@20℃] |
35 |
Young’s modulus [kN/mm2] | 130 |
Poisson’s ratio | 0.33 |
Mechanical properties
Temper | Tensile strength [N/mm2] |
0.2 % yield strength (typical value) [N/mm2] |
Elongation [%] |
Vickers hardness [HV] |
---|---|---|---|---|
1/2H | 500-570 | 525 | 5 Min. | 155-180 |
H | 540-620 | 565 | 4 Min. | 160-195 |
EH | 580-660 | 600 | 3 Min. | 180-215 |
SH | 630-730 | 630 | 3 Min. | 190 Min. |
Bending workability (W bend, bending width=10mm)
Temper | MBR/t | |
---|---|---|
Good Way | Bad Way | |
EH | 0 | 0 |
*Please note that the values in the table are reference values and are subject to change without notice.